Boiling Process

  1. To a clean beaker, add 1.5g of sodium chloride, 1.464 g of Span 60, and 1.288 g of TPGS in 50mL of PBS, and a stirrer bar.
    • This will result in 50 mL of solution, can multiply each ingredient by 2 to get 100 mL, and so on.
    • The smaller the pieces of TPGS, the less time for it to melt


  1. Cover this beaker with aluminum foil and put a piece of “autoclave” tape on the foil.


  1. Heat/stir this beaker (not too hot) until you see it begin boiling. 


  1. Let the solution boil until Span and TPGS completely melt/dissolve, approximately 1-2 hours.

  1. Autoclave for approximately 35 min. This reduces Span60 particle size.  ***